Tira de acero inoxidable
-
Hoja de acero inoxidable
-
Placa de acero inoxidable
-
tubería de acero inoxidable
-
Barra de acero inoxidable
-
Bobina de acero galvanizada
-
Placa de acero
-
barra redonda de acero
-
aleación de níquel
-
Tubería de acero inconsútil
-
Haz de acero inoxidable
-
Hoja de la placa de cobre
-
Barra redonda de cobre
-
stainless steel round bar
-
stainless steel channel bar
-
stainless steel angle bar
-
stainless steel coil strip
-
stainless steel flat bar
-
stainless steel circle
-
Pipe Fitting
-
Water Ripple Stainless Steel Sheet
-
Nickel Alloy and Super Alloy
-
cold rolled steel coil
-
copper
-
Nickel Base Alloy Products
-
Others
-
Raian IonescuCalidad material muy buena. tenemos cooperar más de 10 años. Negocian clases de las porciones de material de acero. Toda la calidad material buena. Ellos deber para toda la calidad material. Estamos acepillando para continuar cooperando con ellos en el futuro
Hastelloy C-22 Nickel Alloy Plate & Round Bar with Cold-Drawing Technique and Polished Surface in OD 6-630mm
| Modelo NO. | Hastelloy C-22 | Forma | Departamento |
|---|---|---|---|
| Técnica | Dibujo en frío | Tratamiento superficial | Pulido |
| Especificación | DE 6-630 mm | Capacidad de producción | 50000KGS |
| Contenido de níquel | Balanza | contenido del cromo | 20,00-22,50% |
| Contenido de molibdeno | 12,50-14,50% | Contenido de hierro | 2.00-6.00% |
| Contenido del tungsteno | 2,50-3,00% | Contenido de cobalto | ≤2,50% |
| Contenido de carbono | ≤0,10% | Contenido de silicio | el ≤0.08% |
| Contenido del manganeso | ≤0.50% | ||
| Resaltar | Cold-Drawing Hastelloy C-22,Polished Nickel Alloy,OD 6-630mm Corrosion Resistant Alloy |
||
Hastelloy C-22 is one of the most widely used nickel-chromium-molybdenum-tungsten alloys. It offers superior resistance to both uniform and local corrosion, making it suitable for various mixed industrial chemicals. HC-22 provides better corrosion resistance than other Ni-Cr-Mo alloys, including C-276, C-4, and 625. C-22 alloys also feature excellent weldability.
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 20.00-22.50 |
| Molybdenum (Mo) | 12.50-14.50 |
| Iron (Fe) | 2.00-6.00 |
| Tungsten (W) | 2.50-3.00 |
| Cobalt (Co) | ≤2.50 |
| Carbon (C) | ≤0.10 |
| Silicon (Si) | ≤0.08 |
| Manganese (Mn) | ≤0.50 |
| Phosphorus (P) | ≤0.02 |
| Vanadium (V) | ≤0.35 |
- 100% PMI, Spectro Chemical Analysis Test for Raw Material
- 100% Dimension & Visual Examination
- Mechanical Properties Test including Tension Test, Flaring Test (for Seamless tube/pipe), Flange Test (for Welded Pipe & Tube), Hardness Test, Reversed Flattening Test
- 100% Hydrostatic Test or 100% Non-Destructive Test (ET or UT)
- Radiographic Test for Welded Pipe (in accordance with specification, or as agreed between purchaser and vendor)
- Straightness Test (optional)
- Roughness Test (optional)
- Intergranular Corrosion Test (optional)
- Impact Test (optional)
- Grain Size Determinations (optional)
Notes: All test and inspection results must be documented in reports according to standard specifications.