Raian IonescuMaterial quality very good. we have cooperate more than 10 Years. They trade lots kinds of steel material. All material quality good. They duty for all material quality. We are planing continue cooperate with them in the future
Martensitic S41500 Stainless Steel Plate Corrosion Resistant with Superior Mechanical Properties
Contact me for free samples and coupons.
Whatsapp:0086 18588475571
Wechat: 0086 18588475571
Skype: sales10@aixton.com
If you have any concern, we provide 24-hour online help.
x| Products | Stainless Steel Plate | Grade | 415 |
|---|---|---|---|
| Thickness | 1.5-50.0mm | Tech | Cold Rolled,hot Rolled , Forged |
| Width | 1000mm 1219mm 1500mm Or Customs As Request | Surface | 2B NO.1 |
| Standard | ASTM GB JIS EN DIN | MOQ | 1 Ton |
Martensitic S41500 Stainless Steel Plate Corrosion Resistant with Superior Mechanical Properties
Stainless Steel Plate Specifications
| Name | 415 stainless steel Plate |
| Our Grade |
200 Series: 201 202 300 Series: 301 304,304L,304H,309S,310S,314,316L,316Ti,316H,316LN,317L,321,329,347 400 Series: 409L,410,410S,415,416,420,430,431,436L.439,441,443,444,445,446 Super Stainless Steel: 904L,926,254SMO,654SMO,15-5PH,17-4PH,17-7PH.etc Nickel Alloy: C276, C22,G35,Alloy X,Monel 400,K500,Inconel 600,601,617,625,718,Incoloy 800,800H,800HT,825.etc |
| Technique | Hot Rolled, Cold Rolled,Forged |
| Standard | JIS, AISI, ASTM, DIN, TUV, BV, SUS, etc |
| Thickness | 0.1 – 80.0mm |
| Width range | 10mm – 2000mm |
| Length | Customized |
| Finish | 2B, BA, No.4, 8k, Brushed,Hairline,PVD Coating,Sandblasted |
| Service | Laser Cutting, Bending |
| Sample | Available |
Introduction
Why Choose Martensitic S41500?
- ✅ High Strength: Tensile strength ≥790 MPa after standard heat treatment
- ✅ Excellent Toughness: Charpy impact energy ≥47 J at –20°C
- ✅ Good Weldability: Low carbon (≤0.06%) minimizes cracking risk
- ✅ Moderate Corrosion Resistance: Performs well in freshwater, steam, and mildly acidic environments
- ✅ Precipitation-Hardenable: Achieves peak properties through simple thermal treatment
Chemical Composition (ASTM A240 Type 415 / UNS S41500)
| Element | Content (%) – Typical Range | ASTM A240 Limit |
|---|---|---|
| Carbon (C) | ≤ 0.06 | Max 0.06 |
| Chromium (Cr) | 11.5 – 14.0 | — |
| Nickel (Ni) | 3.5 – 5.5 | — |
| Molybdenum (Mo) | 0.50 – 1.00 | — |
| Manganese (Mn) | 0.50 – 1.00 | Max 1.00 |
| Silicon (Si) | ≤ 0.60 | Max 0.60 |
| Phosphorus (P) | ≤ 0.030 | Max 0.030 |
| Sulfur (S) | ≤ 0.030 | Max 0.030 |
Mechanical Properties (After Heat Treatment – H1025 Condition)
| Property | Minimum Value |
|---|---|
| Tensile Strength | 790 MPa (115 ksi) |
| Yield Strength (0.2% offset) | 620 MPa (90 ksi) |
| Elongation | ≥ 15% |
| Reduction of Area | ≥ 45% |
| Hardness | 28–34 HRC |
| Charpy V-Notch Impact (–20°C) | ≥ 47 J (35 ft·lbf) |
Note: Heat treatment is essential to achieve these properties. Common tempers include:
- H1025: Standard for turbine applications (550°C/1025°F aging)
- H1150D: Dual tempering for maximum toughness in low-temperature or sour service
Corrosion Resistance Performance
- ✅ Freshwater & Steam: Excellent long-term stability—ideal for hydro turbines
- ✅ Mild Acids & Alkalis: Suitable for chemical processing equipment
- ✅ Atmospheric Exposure: Resists rusting better than carbon steel
- ⚠️ Seawater/High Chlorides: Not recommended without protective coating
Product Offerings & Custom Capabilities
| Feature | Specification |
|---|---|
| Standard | ASTM A240/A240M Type 415 |
| UNS Number | S41500 |
| Common Names | Type 415, F6NM (cast equivalent), 1.4313 (EN), X3CrNiMo13-4 |
| Form | Hot-rolled plate, forged plate, precision blanks |
| Thickness Range | 6 mm – 150 mm (standard); up to 500 mm via forging |
| Max Dimensions | 3000 mm (W) × 12,000 mm (L) |
| Surface Finish | As-rolled, pickled, 2B, machined |
| Certification | EN 10204 3.1 MTR, PMI, UT (ASTM A435), impact test reports |
| Value-Added Services | Laser/waterjet cutting, CNC milling, drilling, beveling, surface grinding, stress relieving |
Comparison with Other Stainless Grades
| Property / Grade | S41500 (Martensitic) | 316L (Austenitic) | 410 (Martensitic) | 2205 (Duplex) |
|---|---|---|---|---|
| Tensile Strength | 790 MPa | 515 MPa | 520 MPa | 620 MPa |
| Yield Strength | 620 MPa | 205 MPa | 290 MPa | 450 MPa |
| Weldability | Good (low C) | Excellent | Poor | Moderate |
| Corrosion Resistance | Moderate (freshwater) | Excellent | Low | Very Good |
| Cost | Medium | High | Low | High |
| Best For | Turbines, shafts | Chemical tanks | Cutlery, fasteners | Offshore pipes |
Key Applications
- Hydroelectric Power: Runner blades, guide vanes, shafts, crown rings
- Oil & Gas: Valves, pump components, downhole tools (NACE-compliant when H1150D treated)
- Marine Engineering: Propeller shafts, rudders, seawater pumps (in low-chloride zones)
- Industrial Machinery: High-wear plates, gears, and structural supports
- Defense & Aerospace: Landing gear fittings, actuator housings
Technical Support & Compliance
- ASTM A240/A240M (plate specification)
- ASTM A751 (chemical analysis)
- NACE MR0175/ISO 15156 (for sour service, with proper heat treatment)
- EN 10088-3 / 1.4313 (European equivalence)
- Welding procedure recommendations (WPS support)
- Heat treatment guidelines
- Material selection consulting
Frequently Asked Questions (FAQ)
A: Yes—it’s martensitic and therefore ferromagnetic, which can be advantageous for certain sensors or lifting applications.
A: Not recommended. As-rolled S41500 lacks required strength and toughness. Heat treatment (e.g., H1025) is mandatory for structural use.
A: Nearly identical chemistry. CA6NM is the cast version (ASTM A743), while S41500 is wrought plate (ASTM A240). Use S41500 for rolled/forged plate applications.
A: Yes—no minimum order. We cut plates to your exact size, even for prototypes.